Amazing results from Li-or, who with help from the group, rapidly sintered an undoped alumina green body she fabricated by slip-casting.  Sintering at 1600C for 3 minutes resulted in a 92% dense body.

Amazing results from Li-or, who with help from the group, rapidly sintered an undoped alumina green body she fabricated by slip-casting.  Sintering at 1600C for 3 minutes resulted in a 92% dense body.

SEM micrograph of rapidly sintered alumina